About sublimation offset ink imprinted drying slowly

After the imprinted which is transferred from the sublimation offset printing plates to the paper by the rubber cloth, generally requirements for within 4 hours which is drying, in order to facilitate the next color printed or finished product testing and shipped out of the factory. Imprinted drying have three aspects factor. And many reasons for caused by imprinting not dry, for example:

  Paper’s PH value is acidic that below 6.

  Large of water and ink on the plate, cause serious ink emulsification.

  Workshop’s temperature is low, relative humidity is higher than 75%.

  The absorbency of paper is poor.

  Too much additive is mixed with ink, such as varnish and viscosity reducer.

  Usage amount of liquid driers is too little.


FLYING Sublimation Printing Material Co., Ltd

Skype : sublimationinks

Tel : 0086-373-7185885

Fax : 0086-373-2116885

Mobile : 0086-15993070542

Email : [email protected]

qqbra.cn/eng

www.sublimeinks.com/eng


 IMG_2064_副本

 dab9364374eb199fc665ff19f833070c_副本

 Dye offset printing ink

More Sharing ServicesShare Share on facebook Share on myspace Share on google Share on twitter

skype